1#5 100 m3 Blast Furnace in Braised Furnace 94 Hours Operation Practice in Shandong SteelZHANG Shouliang1-3,7
Reason Analysis and Technology Improvement on the Cold Drawing Fracture of 55 Round BarGUO Fajun, LI Xiangcai, ZHANG Linlin, CUI Jianhai, ZHANG Zhitao4-7
Cross Section Modification and Production Practice of Beam Blank CasterWU Xupeng, GAO Zhibin, HOU Guangda, LIU Wenping, LIU Zhongjian8-10
Cause Analysis of Bending Cracking of 440 MPa Cold Rolled Steel StripWEI Bingbing, SUN Qian, PAN Aidong, LIU Haibo, LI Yan11-12,15
Low-cost Production Practice of High Carbon Steel in Thin Slab Continuous Casting and Rolling Production LineFU Youpeng, ZHENG Wanren, ZHOU Yongzhi, LIU Lin, WANG Tao13-15
Reason Analysis and Improvement Measures for Nonconforming Flaw Detection at 1/4 Thickness of Bridge PlateCHEN Jianchao, YUE Tumin, CHEN Hao16-18
Flaw Defection Analysis and Improvement Measures of Cutting Tool Steel PlatOU Yangyu, MA Xin, YU Hao, ZHEN Xingang, LIU Zhenhua21-23
Microstructure and Properties of Layers Fabricated by Laser Cladding of Ni-Fe-Cr-C-B Alloy PowdersXUE Xiaojun, QU Haitao, LI Lunxiang, CHEN Xiaoyong, MU Zonghao, LIU Liqian24-27,31