Testing and evaluation methods of steel pipes for hydrogen transmission pipelines
SUN Hong
Abstract:Hydrogen exhibits extremely high permeability and typically degrades metal it comes into contact with.Test and evaluation methods for hydrogen-induced damage in materials have been developed at home and abroad,but the results often differ,or even contradict each one another,due to variations in hydrogen permeation methods,specimen types,test conditions,and testing procedures.This study reviews relevant testing and evaluation methods and testing data for steel pipes used in hydrogen transmission pipelines.Research findings indicate that different hydrogen charging conditions,specimen types,and other factors have a significant impact on the evaluation results of Slow Strain Rate Testing(SSRT).It is recommended that SSRT in a hydrogen environment should specify the specimen type and dimensions according to service conditions.Alternatively,specimens retaining the original surface may be used,and the strain rate range in tensile testing should be narrowed.The hydrogen environment has a significant impact on the plasticity and fatigue crack propagation rate of the metallic materials in contact with it.Appropriate fracture toughness indicators should be selected based on the type of metallic materials,with crack tip opening displacement being suitable for low-strength steel pipes.The fatigue characteristics of hydrogen transmission pipelines were calculated and acceptance criteria for indicators such as fatigue crack propagation rate and fatigue life were proposed based on actual operational pipelines.The study results provide reference for the pipeline construction.
Keywords:Hydrogen transmission pipelinesFracture toughnessFatigue lifeHydrogen environmentSSRT
Publication Date:2025-10-25
Online Publishing Date:2026-11-11(First online date of this platform, not the publication date of the document)
Pages:9( 74-82 )
Natural Gas and Oil

Natural Gas and Oil

ISTIC
ISSN:1006-5539
Year, Vol.(Issue):2025,43(5)