Rapid Reblowing of Angang's No.6 BF Condition after Short Term Damping-downNIU Wei-jun, ZHANG Xiao-liang, LI Hong-fei, TANG Li-xia7-8
Production Practice of Decreasing Pig Iron Silica Content of No.1 350 m3 Blast FurnaceJI Yong-jie, WANG You-fu, LUO Jian-feng, JI Ming-song, ZHANG Xiu-hai9-10
Process Development and Application of Melting Low-carbon and Low-silicon Steel Grade in JigangZHENG Shu-sheng, TANG Li-dong, ZHANG Mao-cun11-13
Production Practice of Decreasing the Surface Longitudinal Crack of Continuously Casting SlabDONG Jin-wu, LIU Hong-bo, GAO Long-yong, ZHANG Song-ling13-15
Reason Analysis and Countermeasures of Mould Slag Entrapment in the Production of Steel C72DALIU Xin16-17
Reason Analysis and Countermeasures of Influencing the Service Life of Slab CCM SegmentZHOU Ning18-20
Practice of Producing 1.8mm × 800mm Strip Steel by 950 Hot Tandem MillLI Zhou, WANG Ji-quan, ZHANG Wu-yin, CAO Xu-dong23-24