Production Practice of Adding Economic Iron Ores in Jinan Steel's 320 m2 Sintering MachineHUA Xu-jun, SHEN Ai-min, ZHOU Chang-qiang, BAO Yang1-3,6
Low Carbon and Deep-bed Sintering Practice of Laiwu Steel's 265 m2 Sinter MachineWANG Wei, WANG Ke, CHENG Wen-zhang, LI Lian-hai, MA Qing-guo4-6
Smooth Operation Practice of Laiwu Steel' s 3 200 m3 BF after Starting-upQIU Guo-xing, WANG Lian-chang, TANG Deng-jun, LI Hai-ming7-9
Control Measures of Taphole Splashing in Jinan Steel' s 3 200 m3 BFZHANG Xiao-wei, WANG Li-bo, DU Min-qing10-11
Analyses of the Slopping Cause of 90 t Converter in Laiwu Steel and the CountermeasuresZHENG Jie12-13
Analysis and Control of the Nitrogen Content Increasing in Steelmaking and Casting ProcessesZHANG li-biao, CHEN Chuan-lei, CHEN Chang-yi, GAO Long-yong, YIN Wei-ping14-15
Application of High Radiant Coating Technology in Jinan Steel's BF Hot-blast StovesZHOU Hui-min, ZHANG Rui-tang, LI Bing-lai, WANG Lian-jie, LIU Yi-zhou18-19,21
Process Practice of Kalugin Top-combustion Stove Long-term Heat Preservation in Laiwu SteelTANG Ji-xue20-21
Failure Analysis and Improvement of the CDQ Coke Rotating-cansSHAN Xiao-wei, WANG Yong-li, ZHOU Yong, ZHANG Shuai22-23