Study on Inclusion Control for Ultra Low Oxygen GCr15 Bearing Steel
FU Pengchong
LI Wenshuang
ZHU Linlin
Abstract:By taking a series of measures such as controlling inclusion source, optimizing deoxidization technology, using high basicity refining slag, modifying the inclusions, improving soft blowing process and protective casting, Xiwang Special Steel achieved smelting of ultra low oxygen bearing steel. Total oxygen content T[O]≤8×10-6,B-type inclusion (Heavy) level 0-0.5, (Thin) level 0-1.0, D-type inclusion (Heavy) level 0-0.5, (Thin) level 0-0.5.
Keywords:bearing steelinclusionrefiningoxygen content
Publication Date:2015-01-01
Online Publishing Date:2026-05-22(First online date of this platform, not the publication date of the document)
Pages:3( 23-25 )
Shandong Metallurgy

Shandong Metallurgy

ISSN:1004-4620
Year, Vol.(Issue):2015,(6)