Solutions to sulfide high temperature corrosion problem in W flame boiler
ZHANG Feng
SONG Libin
YAN Junshan
TIAN Zhanjun
Keywords:W-shape flame boilerhigh temperature corrosionlow-nitrogen combustioncombustion adjustmentreducing atmosphere
Publication Date:2016-01-01
Online Publishing Date:2025-08-15(First online date of this platform, not the publication date of the document)
Pages:7( 41-47 )
Clean Coal Technology

Clean Coal Technology

ISTIC
ISSN:1006-6772
Year, Vol.(Issue):2016,22(5)